The description of Type 3 shall not be increased to 95% tin. Concern is that some manufacturers will change their tin-lead composite to a higher tin percentage. ESCC requires special precautions for 85% to 95% tin. Therefore, DLR proposal is to add a new type 19 for the relay manufacturers' SnPb with a tin percentage between 85% and 95%. Furthermore, solder behavior of 95% Sn is slightly different to eutectic composition.